Item No. |
Type |
Tectorial Membrane Apperance Tectorial Membrane Weight(g/m2) |
Use Condition |
Features |
Use Method |
Trough Dosage |
Use Temperature(℃) |
Treating Time (min) |
TL-3108 |
Zinc Phosphate |
Gray
white
5~10 |
Dipping |
50KG/T |
70~80 |
3~10 |
Suitable for the drawing of steel tube and cold forging and deep dawning of steel plate. |
TL-3109 |
Zinc Phosphate |
Gray
white
5~10 |
Dipping |
100KG/T |
70~80 |
2~7 |
Suitable for drawing and cold rolling of wire. |
TL-3205 |
Zinc Calcium Phosphate |
Grey
black
5~10 |
Dipping |
70KG/T |
80~90 |
8~10 |
Drawing of steel tube and deep dawning of steel plate. It has the rust prevention function. |
TL-3208 |
Zinc Phosphate |
Gray
white
5~10 |
Dipping |
60KG/T |
60~85 |
8~10 |
Used for phosphating treatment before cold plastic working such as cold plastic working and the dawning of wire. |
TL-3909 |
Grey
5~10 |
Dipping |
30KG/T |
90~98 |
3~6 |
Suitable for the phosphating treatment of aluminium pumping tube and aluminium forging technics. |